3M 9082

Harmonization Code : 3907.30.00.40 | Epoxy Mold Compounds containing by weight more than 70 % silicon dioxide

3M 9082

Main features

  • 177 deg C Long-Term Bonding
  • Low-Outgassing Electronics Adhesion
  • Thin 0.05 mm Transfer Layer

Product Description

3M Ultra High Temperature Adhesive Transfer Tape 9082 is a clear 0.05 mm acrylic adhesive transfer tape with a 0.08 mm 55# densified-kraft release liner for thin, high-temperature bonding in electronics and automotive assemblies. The low-outgassing adhesive system retains measurable adhesion through elevated-temperature testing: 180 deg peel adhesion is 8.8 N/cm at 23 deg C and 5.3 N/cm at 177 deg C on aluminum-foil-backed specimens. Long-term temperature resistance is 177 deg C and short-term resistance is 280 deg C. The construction is intended for assemblies that combine thin bondlines with elevated processing or operating temperatures.

Key features

  • High-temperature acrylic bonding: Long-term temperature resistance reaches 177 deg C, with short-term exposure resistance to 280 deg C.
  • Low-outgassing thin transfer layer: The clear 0.05 mm adhesive layer provides a thin bonding profile for electronics and automotive assemblies.
  • Measured elevated-temperature adhesion: Peel adhesion remains measurable through 230 deg C testing, with 5.3 N/cm recorded at 177 deg C.

Applications

Applications include automotive under-hood bonding, flexible printed circuit and FR-4 attachment, electronics and heat-sink bonding, and solder-reflow process assemblies.

Product Family

3M 9082

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

Technical Specifications

No specifications available.

Additional Information

Technical properties

As-supplied / before-processing properties

PropertyValueUnitMethod / condition
ColorClearAs supplied
Density0.98g/cm^3Typical
Adhesive typeAcrylic adhesive systemHigh-temperature adhesive
Adhesive thickness0.05mmASTM D3652; typical
Liner55# densified kraftWhite with green 3M print
Liner thickness0.08mmTypical
Technical properties

After-processing / final-state properties

PropertyValueUnitMethod / condition
180 deg peel adhesion at 23 deg C8.8N/cmASTM D3330; 2 mil aluminum foil backing; typical
180 deg peel adhesion at 177 deg C5.3N/cmASTM D3330; specimen conditioned 2 min at temperature; typical
Overlap shear strength at 23 deg C620kPaASTM D1002 / ISO 4587; stainless steel; typical
Long-term temperature resistance177deg CDays to weeks; typical
Short-term temperature resistance280deg CMinutes to hour; typical
Dielectric strength at 23 deg C1200VASTM D149; typical

Leading Brands Trust in Our Products and Services

  • Jabil
  • Linxens
  • Magna
  • Medtronic
  • NXP
  • Philips
  • Semikron
  • Teledyne
  • Thales
  • Vishay
  • ZF
  • AMS
  • Apple
  • Audi
  • Broadcom
  • Borgwarner
  • Bosch
  • Eaton
  • Henkel
  • Honeywell
  • Hysol
  • Intel
Products that Perform|Knowledge that Serves|Service that Delivers